Creep testing machine
Make : M/s. Spranktronics, Bangalore, India.
Application : Creep tests of polymers under tensile mode
Specification :
Load capacity : up to 100 kg
Data Acquisition System : Measurement of load, displacement , temperature with hardware processing unit and time.
Software : Lab view software provides online plots of temperature-time vs load/displacement
Temperature range of the oven : 25°C to 250°